|a Vplyv tepelného spracovania na mikroštruktúru, mikrotvrdosť a odolnosť proti korózii ZE41 Mg zliatiny
|y slo
|
245 |
0 |
0 |
|a Effect of heat treatment on microstructure, microhardness and corrosion resistance of ZE41 Mg alloy
|c U. Syam Prasad ... [et al.]
|
300 |
|
|
|b Obr., tab.
|
504 |
|
|
|a Bibliogr. odkazy
|
546 |
|
|
|a Res. angl.
|
650 |
0 |
4 |
|a zliatiny horčíka
|
650 |
0 |
4 |
|a tepelné spracovanie
|
650 |
0 |
4 |
|a korózna odolnosť
|
650 |
0 |
4 |
|a tvrdosť
|
700 |
1 |
|
|a Syam Prasad, U.
|4 aut
|
700 |
1 |
|
|a Kondaiah, V. V.
|4 aut
|
700 |
1 |
|
|a Akhil, K.
|4 aut
|
700 |
1 |
|
|a Vijay Kumar, V.
|4 aut
|
700 |
1 |
|
|a Nagamani, B.
|4 aut
|
700 |
1 |
|
|a Jhansi, K.
|4 aut
|
700 |
1 |
|
|a Ravikumar Dumpala
|4 aut
|
700 |
1 |
|
|a Venkateswarlu, B.
|4 aut
|
700 |
1 |
|
|a Ratna Sunil, B.
|4 aut
|
773 |
0 |
|
|t Koroze a ochrana materiálu
|g Roč. 63, č. 2 (2019), s. 79-85
|x 1804-1213
|
958 |
|
|
|a NB
|
974 |
|
|
|a DZA
|
992 |
|
|
|a RBX
|
BAS |
|
|
|
852 |
|
|
|a SVKKK
|b BIB
|
856 |
4 |
1 |
|u https://content.sciendo.com/view/journals/kom/63/2/article-p79.xml
|
998 |
|
|
|a HUT
|